Well-dispersed cerium-doped Y2SiO5 (Ce:YSO) phosphor particles with spherical morphology and good luminescence intensity have been achieved by a solvothermal method with ethanol and water as solvent media. X-ray diffraction, Fourier transform infrared spectroscopy, fluorescence spectrophotometry and transmission electron microscopy were employed to characterize the as-synthesized Ce:YSO precursor and powders. The results showed that pure-phase Ce:YSO powders with a mean particle size of about 162 nm were accurately available at 310°C and above. The fluorescence ability and persistent luminescence decay properties of the Ce:YSO powders were also studied, and the excellent fluorescence properties could be attributed to the homogeneous Ce:YSO particles obtained through the solvothermal method.
Subject
Materials Chemistry,Metals and Alloys,Physical and Theoretical Chemistry,Condensed Matter Physics
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献