Abstract

Abstract The aim of this contribution is to review cases of repeated snap ring failures in large gas turbine engine service due to intergranular attack, or intergranular corrosion, IGC, and to shed some light on metallurgical aspects of the wet corrosion resistance of the subject high-alloy martensitic stainless chromium steel X39CrMo17-1, DIN 1.4122. It is important to note that only snap rings, a.k.a. retaining rings for bores or Seeger rings, were affected by those failures, namely fractures resulting from intergranular attack (IGA, Kornzerfall). It was determined that the metallurgical root cause of failure was sensitization, resulting from secondary chromium carbide precipitation at grain boundaries (GB), and the ensuing chromium depletion in narrow bands adjacent to the GB, which rendered the matrix there sensitive to selective corrosion (the chromium content in these narrow seams, measuring only a few 10 nm in width, drops below the corrosion resistance threshold of ca. 10.5 %). Snap rings, as the name suggests, require a certain “snappiness” to serve their purpose. It is because of this requirement that all snap rings that experienced failures in the field were heat treated per DIN EN 10088-2, providing for a low tempering temperature of max. 250 °C, leading to a relatively high hardness of ca. 580 HV 10, providing said “snappiness”. It turned out that the microstructure resulting from this heat treatment (H/T) is sensitized, rendering the material sensitive to IGA. To the knowledge of the authors, no other components made of this martensitic stainless chromium steel are given this H/T, but rather a high-temperature tempering of 650 °C–750 °C per DIN EN 10088-3, producing a lower hardness in the order of ca. 300 HV 10 and largely a lack of “snappiness”, the latter being not required by those non-snap ring applications. Metallurgically, it became clear that high-temperature tempering per DIN EN 10088-3 eliminates sensitization by “backfill” diffusion of chromium from the non-depleted matrix into formerly depleted regions next to GB. It was therefore decided in the authors’ organization to eliminate X39CrMo17-1 per DIN EN 10088-2 as a possible material selection. The metallurgical investigations described in this contribution corroborate and support this decision.

Publisher

Walter de Gruyter GmbH

Subject

Metals and Alloys,Mechanics of Materials,Condensed Matter Physics,Electronic, Optical and Magnetic Materials

Reference30 articles.

1. VDI-Richtlinie 3822, Part 3: March 2007: Failure analysis – Failures caused by corrosion in electrolytes. Beuth-Verlag GmbH, Berlin, Düsseldorf 2007.

2. Maier, F.; Opielka, H.: Interkristalline Korrosion vonSicherungsringenaus 1.4122(X39CrMo17-1). Prakt. Met. Sonderband 36 (2004), S. 365–366. DOI: 10.5840/intstudphil2004361109

3. Lange, G. (Hrsg.): Systematische Beurteilung technischer Schadensfälle. 3. Auflage, DGM, 1992.

4. ASM Handbook, Volume 11: Failure Analysis and Prevention. 6. Auflage, ASM International, 1998.

5. Handbook of Case Histories in Failure Analysis, Volume 1. ASM International, Materials Park, OH, Third Printing 2002.

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3