AbstractTitanium is used in many areas due to its excellent mechanical, biological and corrosion-resistant properties. Implants often have thin and filigree structures, providing an ideal application for fine cutting with laser. In the literature, the main focus is primarily on investigating and optimizing the parameters for titanium sheets with thicknesses greater than 1 mm. Hence, in this study, the basic manufacturing parameters of laser power, cutting speed and laser pulse of a 200 W modulated fiber laser are investigated for 0.15 mm thick grade 2 titanium sheets. A reproducible, continuous cut could be achieved using 90 W laser-power and 2 mm/s cutting-speed. Pulse pause variations between 85 and 335 μs in 50 μs steps and a fixed pulse width of 50 μs show that a minimum kerf width of 23.4 μm, as well as a minimum cut edge roughness Rz of 3.59 μm, is achieved at the lowest pulse pause duration. An increase in roughness towards the laser exit side, independent of the laser pulse pause duration, was found and discussed. The results provide initial process parameters for cutting thin titanium sheets and thus provide the basis for further investigations, such as the influence of cutting gas pressure and composition on the cut edge.
Funder
Regensburg Center of Health Sciences and Technology
Regensburg Center of Biomedical Engineering
Bayerische Forschungsstiftung
Ostbayerische Technische Hochschule Regensburg
Publisher
Springer Science and Business Media LLC
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献