Abstract
Abstract
Objectives
Evaluation of cumulative survival and complication rate of monolithic lithium disilicate inlays and partial crowns performed by supervised undergraduate students up to 8.3 years of clinical service.
Materials and methods
In this retrospective clinical study 143 lithium disilicate posterior restorations (IPS e.max Press) were examined according to the FDI criteria. A standardised questionnaire was used to determine patient satisfaction. The aesthetic outcome was evaluated by dentists and dental technicians using intraoral photographs. Data were descriptively analysed. Cumulative survival and success rates were calculated using Kaplan–Meier estimation.
Results
The cumulative survival rate of lithium disilicate restorations was 97.5% after a mean service time of 5.9 years and 95.0% after 8.3 years. The cumulative success rate decreased from 94.4% after 5.9 years to 30.7% after 8.3 years. Repairs were required for 7 restorations (4.9%), and 5 (3.5%) were classified as failures. The results of the questionnaire indicate a high level of patient satisfaction. The subjective aesthetics were assessed more critically by dental technicians compared to dentists.
Conclusion
Lithium disilicate posterior restorations survived successfully up to 8.3 years when carried out by undergraduate students.
Clinical relevance
Pressed lithium disilicate glass ceramic inlays and partial crowns are reliable treatment options in posterior teeth.