1. S. S. Hecker and J. R. Morgan, “Effect of strain rate on the tensile properties of α-and γ-stabilized plutonium,” in:Plutonium 1975 and Other Actinides, North-Holland Publ. Comp., Amsterdam (1976), pp. 697–708.
2. M. D. Merz, “Strength differential effect in α-Pu,”Metall. Trans.,4, No. 4, 1186–1188 (1973).
3. S. Beitscher, “The tensile behavior of Pu/1 wt.% Ga at −60, 30, and 77°C,”J. Nucl. Mater.,24, No. 1, 113–117 (1967).
4. Yu. V. Bat'kov, V. K. Golubev, S. A. Novikov, et al., “Fracture of plutonium and its alloy with 1.6 wt.% gallium under impact loading,”Vopr. Atom. Nauki Tekh., Ser. Fiz. Yadernykh Reaktorov,1, 40–42 (1991).
5. M. D. Merz, J. H. Hammer, and H. E. Kjarmo, “Sound velocity and elastic moduli in α-plutonium at pressures to 50 kbar,” in:Plutonium 1975 and Other Actinides, North-Holland Publ. Comp., Amsterdam (1976), pp. 567–571.