1. S. Ya. Yarema, “On the stabilization of stresses in the vicinity of the tip of a growing crack,”Probl. Prochn., No. 8, 15–19 (1975).
2. J. M. Bloom, “Single-edge crack in rectangular sheet subjected to end rotations,”Appl. Mech.: Trans. ASME, Ser. E. 33, No. 3, 243–246 (1966).
3. V. I. Pokhmurskii, N. M. Kundrat, L. M. Bilyi, et al., “On the constancy of the stress intensity factor at the tip of a crack in the process of its propagation in a rectangular plate,”Probl. Prochn., No. 12, 59–62 (1984).
4. L. M. Bilyi,Change in Cyclic Crack Resistance of Steels under Electrolytic Hydrogenation [in Russian], Author's Abstract of the Candidate-Degree Thesis (Technical Sciences), L'viv (1989).
5. R. A. Oriani, “Hydrogen embrittlement of steel,”Ann. Rev. Mater. Sci.,8, 327–357 (1978).