1. W.A. Maxwell, “Properties of Certain Intermetallics as Related to Elevated-Temperature Applications. I—Molybdenum Disilicide,” report no. NACA RM E9G01 (1949).
2. W.A. Maxwell, “Some Factors Affecting Fabrication and High-Temperature Strength of Molybdenum Disilicide,” report no. NACA RM E52B06 (1952).
3. R.A. Long, “Fabrication and Properties of Hot-Pressed Molybdenum Disilicide,” report no. NACA RM E50F22 (1950).
4. E. Fitzer, O. Rubisch, J. Schlichting and I. Sewdas, “The Recrystallization Behavior of Sintered MoSi!!!2!! Without and With SiC and Al!!!2!!O!!!3!! Additions Between 1500 and 1700°C and the Effect of Structural Changes on the Bend Strength,” Sci. Ceram., XVIII(6) (1973).
5. W.S. Gibbs, J.J. Petrovic and R.E. Honnell, “SiC Whisker-MoSi!!!2!! Matrix Composites,” Ceram. Eng. Sci., 8 (1987), p. 645.