Abstract
AbstractAccident tolerant fuel (ATF) cladding is a new type of nuclear fuel cladding designed to improve the safety and performance of nuclear reactors. In this paper, the kinetics and degradation mechanisms during high-temperature oxidation in steam of the three most promising ATF cladding materials, i.e., chromium-coated zirconium alloys, FeCrAl alloys, and silicon carbide-based composites, are described. Each system has its own degradation mechanisms leading to different maximum survival temperatures. After providing general information and data to understand the oxidation and degradation processes, illustrative examples obtained at the Karlsruhe Institute of Technology are given for each type of cladding. The maximum temperatures at which the barrier effect of the cladding can be maintained for a reasonable period of time during nuclear accident scenarios are 1200–1300 °C for Cr-coated Zr alloys, 1400 °C for FeCrAl alloys, and 1700 °C for SiC-based composite claddings.
Funder
Karlsruher Institut für Technologie (KIT)
Publisher
Springer Science and Business Media LLC
Reference98 articles.
1. V. Inozemtsev, and V. Onufriev, in LWR Fuel Performance Meeting, Top Fuel 2013 (2013).
2. M. Steinbrück, M. Große, L. Sepold, and J. Stuckert, Nuclear Engineering and Design 240, 1714 (2010).
3. M. Steinbrück, in Encyclopedia of Materials: Metals and Alloys, vol. 1, ed. F. G. Caballero (Elsevier, Oxford, 2022), p. 454.
4. S. Zinkle, K. Terrani, J. Gehin, L. Ott, and L. Snead, Journal of Nuclear Materials 448, 374 (2014).
5. B. Pint, K. Terrani, Y. Yamamoto, and L. Snead, Metallurgical and Materials Transactions E 2, 190 (2015).
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献