Abstract
AbstractOxidation of the Fe-base alloy T22 in humid air at 500 °C was investigated. The samples were exposed for up to 1000 h at 1 bar and 20 bar. The influence of three furnace tube materials, alumina, ET45 and quartz glass, on the oxide scale morphology was investigated. Samples and their cross sections were examined using optical microscopy, scanning electron microscopy, electron probe micro analysis and Raman spectroscopy. Multilayered oxide scales consisting of hematite, magnetite and Fe–Cr spinel were found on all samples. However, the composition and morphology of the oxide scales depend on the furnace tube material and on the system pressure. The system pressure is assumed to change the reaction equilibria and adsorption rates. The tube material changed the initial gas composition by formation of volatile Cr species. This volatilization rate increased at higher system pressures.
Funder
DECHEMA-Forschungsinstitut
Publisher
Springer Science and Business Media LLC
Subject
Materials Chemistry,Metals and Alloys,Inorganic Chemistry
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献