Abstract
AbstractHere we present an economical ambient pressure drying method of preparing monolithic silica aerogels from methyltrimethoxysilane precursor while using sodium bicarbonate solution as the exchanging solvent. We prepared silica aerogels with a density and a specific surface area of 0.053 g·cm−3 and 423 m2·g−1, respectively. The average pore diameter of silica aerogels is 23 nm as the pore specific volume is 1.11 cm3·g−1. Further, the contact angle between water droplet and the surface of silica aerogels in specific condition can be as high as 166°, which indicates a super-hydrophobic surface of aerogels.
Publisher
Springer Science and Business Media LLC
Subject
General Chemical Engineering
Reference23 articles.
1. Hüsing N, Schubert U. Aerogels—airy materials: chemistry, structure, and properties. Angewandte Chemie International Edition, 1998, 37(1–2): 22–45
2. Wang C, Okubayashi S. 3D aerogel of cellulose triacetate with supercritical antisolvent process for drug delivery. Journal of Supercritical Fluids, 2019, 148: 33–41
3. Wang C, Liang W, Yang Y, Liu F, Sun H, Zhu Z, Li A. Biomass carbon aerogels based shape-stable phase change composites with high light-to-thermal efficiency for energy storage. Renewable Energy, 2020, 153: 182–192
4. Tsou P. Silica aerogel captures cosmic dust intact. Journal of Non-Crystalline Solids, 1995, 186: 415–427
5. Smirnova I, Gurikov P. Aerogels in chemical engineering: strategies toward tailor-made aerogels. Annual Review of Chemical and Biomolecular Engineering, 2017, 8(1): 307–334