1. Z.X. Dong, G.C. Ji, M.L. Ma, Y.M. Gao, Application of hypereutectic high-chromium cast iron in abrasive wear at elevated temperature. Foundry Technol. 27(1), 4–7 (2006)
2. H. Yan, J.P. Xie, W.Y. Wang, J.W. Li, Optimization of heat treatment process and mechanical properties enhancement of super-high manganese steel. Foundry 55(10), 1067–1070 (2006)
3. A.H. Cai, G.X. Sun, Q.X. Tang, Effect of Cr, Si, Mn and Cu on the corrosive wear resistance of low-medium chromium white cast iron. Develop Appl. Mater. 17(6), 5–8 (2002)
4. J.T.H. Pearce, High-chromium cast irons to resist abrasive wear. Foundryman 95(4), 156–166 (2002)
5. R.W. Durman, D.W.J. Elwell, Morphology eutectic carbide in high chromium white irons. British Foundryman 78, 371–375 (1985)