1. M. L. S. Zappulla and B. G. Thomas, “Surface defect formation in steel continuous casting,” Materials Science Forum, 941, 112–117 (2018); DOI:https://doi.org/10.4028/www.scientific.net/msf.941.112.
2. A. B. Biryukov, Improvement of Thermal Engineering parameters for a System for Producing Continuously-Cast Billets and Heat Treatment: Monograph [in Russian], Nowlidzh (Donetsk section) Donetsk (2013).
3. S. A. Botnikov, Contemporary Atlas for Continuously-Cast Billet defects in Regions fro Occurrence of Breaks in the Crystallized metal Ski [in Russian], Panoram, Volgograd (2011).
4. G. Poltarak, S. Ferro, and C. Cicutti, “Estimation of internal cracking risk in the continuous casting of round bars,” Steel Research International, 88, No. 4, 1600223 (2016); DOI:https://doi.org/10.1002/srin.201600223.
5. A. B. Biryukov, V. V. Kravtsov, I. P. Oleksyuk, and N. A. Ostapenko, “Effective control of secondary cooling zone of high-speed section CBCM,” Metall i Lit’e Ukrainy, No. 7, 21–23 (2010).