1. Shrestha, S., Hodgkies, T., Neville, A.: Erosion–corrosion behavior of high velocity oxy-fuel Ni–Cr–Mo–Si–B coating under high-velocity seawater jet impingement. Wear 259, 208–218 (2005)
2. Chen, H.S., Li, J., Liu, S.H.: Thermal effect at the incipient stage of cavitation erosion on a stainless steel. J. Fluid Eng. 231, 1–3 (2009)
3. Chen, H.: Iridescent rings around cavitation erosion pits on surface of mild carbon steel. Wear 269, 602–606 (2010)
4. Chen, H., Li, J., Chen, D., Wang, J.: Damages on steel surface at the incubation stage of the vibration cavitation erosion in water. Wear 265, 692–698 (2008)
5. Chen, H., Li, J., Chen, D., Wang, J.: Affected zone generated around the erosion pit on carbon steel surface at the incipient stage of vibration cavitation. Chin. Sci. Bull. 53, 943–947 (2008)