1. Liu, W., Zheng, Y.G., Liu, C.S., Yao, Z.M., Ke, W.: Cavitation erosion behavior of Cr–Mn–N stainless steels in comparison with 0Cr13Ni5Mo stainless steel. Wear 254, 713–722 (2003)
2. Mesa, D.H., Garzon, C.M., Tschiptschin, A.P.: Influence of cold-work on the cavitation erosion resistance and on the damage mechanisms in high-nitrogen austenitic stainless steels. Wear 271, 1372–1377 (2011)
3. Qiao, Y.X., Wang, S., Liu, B., Zheng, Y.G., Li, H.B., Jiang, Z.H.: Synergistic effect of corrosion and cavitation erosion of high nitrogen stainless steel. Acta Metall. Sin. 52, 233–240 (2016)
4. Qiao, Y.X., Cai, X., Cui, J., Tang, Y.B., Li, H.B., Jiang, Z.H.: Cavitation erosion properties of a nickel-free high-nitrogen Fe–Cr–Mn–N stainless steel. Mater. Technol. 51, 933–938 (2017)
5. Al-Hashem, A., Caceres, P.G., Abdullah, A., Shalaby, H.M.: Cavitation corrosion of duplex stainless steel in seawater. Corrosion 53, 103–113 (1997)