1. X. Guo, S. Gin, P. Lei, T. Yao, H. Liu, D.K. Schreiber, D. Ngo, G. Viswanathan, T. Li, S.H. Kim, J.D. Vienna, J.V. Ryan, J. Du, J. Lian, and G.S. Frankel, Self-Accelerated Corrosion of Nuclear Waste Forms at Material Interfaces, Nat. Mater., 2020, 19, p 310–316.
2. X. Guo, S. Gin, and G.S. Frankel, Review of Corrosion Interactions Between Different Materials Relevant to Disposal of High-Level Nuclear Waste, npj Mater. Degrad., 2020, 4, p 1–16.
3. Y.S. Li, S.D. Zhang, L. Xian, L.J. Liu, S.G. Tan, H. Zhang, H. Zhou, and D.S. Qie, Progress in Research and Development of Vitrification Technology for High-Level Radioactive Liquid Waste at CIAE, At. Energy Sci. Technol., 2020, 54, p 126–136.
4. K. Xu, International Research Progress on Solidification of Nuclear Waste Glass, Adv. Mater. China, 2016, 35, p 481–487.
5. Q.F. Xu, K. Gao, W. Lv, and X. Pang, Effects of Alloyed Cr and Cu on the Corrosion Behavior of Low-Alloy Steel in a Simulated Groundwater Solution, Corros. Sci., 2016, 102, p 114–124.