1. A. K. Bhaduri, K. Laha, S. K. Albert, T. Jayakuar and S. C. Chetal, Proceeding of 41 st MPA-Seminar, Stuttgart (2015).
2. H. Okada, Y. Sawaragi, F. Masuyama and N. Komai “Mechanical Properties and Microstructure of 0.1C-18Cr-9Cr-3Cu-Nb,N Steel Tube after Long Term Exposures in a Power Boiler” CREEP 7, Proc. Of the 7th International conference on Creep and Fatigue at Elevated Temperatures, The Japan Society of Mechanical Engineers, June 3–8, 2001, NIMS, Tsukuba, Japan.
3. Y. Sawaragi, K. Ogawa, S. Kato, A. Natori and S. Hirano, “Development of the Economical 18-8 Stainless Steel (SUPER 304H) having High Elevated Temperature Strength for Fossil Fired Boilers” The Sumitomo Research, No. 48, January, 1992, Sumitomo Metal Industries, Ltd., Osaka & Tokyo, Japan.
4. “DMV 304HCu” Salzgitter Mannesmamm Stainless Tubes-report