1. V. A. Tsykanov, V. K. Shamardin, A. B. Andreeva, et al., “Physical-metallurgical studies of VK-50 reactor fuel assemblies,” At. Énerg., 56, No. 3, 131–134 (1984).
2. I. M. Smirnov, Distribution of the Elements in Deposits on the Cladding of Fuel Elements in Water-Cooled Nuclear Reactors: Auth. Abstr. Cand. Dissert. Techn. Sci., Ulyanovsk (2011).
3. A. M. Krasnov, V. M. Eshcherkin, V. E. Shmelev, et al., “Processes leading to the concentration of dissolved impurities in coolant (‘hide-out’) on the VK-50 research reactor,” Teploenergetika, No. 7, 18–23 (2002).
4. V. V. Konyashov and A. M. Krasnov, “Experience in operating the VK-50 nuclear reactor with non-hermetic fuel elements,” in: Trudy GNTs RF NIIAR, Dimitrovgrad (2000), Iss. 3, pp. 25–26.
5. A. Garlick. R. Sumerling, and G. Shires, “Crud-induced overheating defects in water reactor fuel pins,” J. Brit. Nucl. Energy Soc., 16, No. 1, 77–80 (1977).