1. M.F. Dodge, H.B. Dong, M. Millititsky, R.P. Barnett, V.F. Marques, M.F. Gittos: Environment-induced cracking in weld joints in subsea oil and gas systems—part 1. 31st International Conference on Ocean, Offshore and Arctic Engineering (OMAE2013).
2. M.F. Gittos and T.G. Gooch: The interface below stainless steel and nickel-alloy claddings, 1992.
3. V. Olden, P.E. Kvaale, P.A. Simensen, S. Aaldstedt, J.K. Solberg: The effect of PWHT on the material properties and micro structure in Inconel 625 and Inconel 725 buttered joints. Canun, Mexico, OMAE, 2003. OMAE 2003–37196.
4. Alexandrov BT, Lippold JC, Sowards JW, Hope AT, Saltzmann DR (2012) Fusion boundary microstructure evolution associated with embrittlement of Ni–base alloy overlays applied to carbon steel. Weld World. doi: 10.1007/s40194-012-0007-1
5. B.T. Alexandrov, J.M. Rodelas, Shu Shi, J.C. Lippold: A new test for evaluation of susceptibility to hydrogen assisted cracking in dissimilar metal welds. NACE International Corrosion Conference and Expo, 51312-01602-SG (2012).AST14 ASTM International: A182/A182M–14: Standard Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service, 2014.