Reference13 articles.
1. Kasuya T (2001) Modelling of trap-controlled hydrogen diffusion in steel. Defect Diff Forum 188–190:115–124
2. Flis-Kabulska I, Zakroczymski T, Flis J (2007) Accelerated entry of hydrogen into iron from NaOH solutions at low cathodic and low anodic polarisations. Electrochim Acta 52(9):2966–2977
3. Choo W, Lee J (1982) Thermal analysis of trapped hydrogen in pure iron. Metall Trans A 13:135–140
4. Swieczko-Zurek B, Sobieszczyk S, Cwiek J, Zielinski A (2006) Evaluation of susceptibility of high strength steels to hydrogen delayed cracking. J Achiev Mater Manuf Eng 18(1–2):243–246
5. Eliaz N, Shachar A, Tal B, Eliezer D (2002) Characteristics of hydrogen embrittlement, stress corrosion cracking and tempered martensite embrittlement in high-strength steels. Eng Fail Anal 9:167–184