1. S. N. Grigoriev, A. N. Krasnovskii, and I. A. Kazakov, “The impact of pre-heating on pressure behavior in tapered cylindrical die in pultrusion of large-sized composite rods,” Adv. Mater. Res., 1064, 120 – 127 (2015); doi:
10.4028/www.sci-entific.net/AMR.1064.120
.
2. S. N. Grigor’ev, A. N. Krasnovskii, and K. V. Kvachev, “Permeation of glass fibers during pultrusion of polymer composite materials,” Steklo Keram., No. 12, 28 – 30 (2014); S. N. Grigor’ev, A. N. Krasnovskii, and K. V. Kvachev, “Permeation of glass fibers during pultrusion of polymer composite materials,” Glass Ceram., 71(11 – 12), 443 – 445 (2014).
3. S. N. Grigor’ev, A. N. Krasnovskii, and I. A. Kazakov, “Effect of preliminary heating of the binder on the quality of glass composite pultrusion rods,” Steklo Keram., No. 8, 36 – 40 (2015); S. N. Grigor’ev, A. N. Krasnovskii, and I. A. Kazakov, “Effect of preliminary heating of the binder on the quality of glass composite pultrusion rods,” Glass Ceram., 72(7 – 8), 299 – 302 (2015).
4. S. N. Grigoriev, A. N. Krasnovskii, and I. A. Kazakov, “The friction force determination of large-sized composite rods in pultrusion,” Appl. Composite Mater., 21(4), 651 – 659 (2014); doi:
10.1007/s10443-013-9360-5
.
5. A. A. Kutin, A. N. Krasnovskii, and I. A. Kazakov, “The fiber orientation angle determination for a composite anisotropic solid rod in pultrusion,” Adv. Mater. Res., 941(26), 2273 – 2278 (2014); doi:
10.4028/www.scien-tific.net/AMR.941-944.2273
.