1. D. Dekate, B.D. Deshmukh, S. Khedkar, Study and minimization of surface defects on bars and wire rod originated in continuous cast billets. Int. J. Mod. Eng. Res. (IJMER) 3(2), 736–738 (2013)
2. J.C. Pandey, M. Raj, P.N. Choubey, Split ends and cracking problem during hot rolling of continuously cast billets. J. Fail. Anal. Prev. 9, 88–96 (2009)
3. E.T. Turkdogan, Consequences of microsegregation during solidification of steel: subsurface-blowhole formation, oxysulfide, and sulfide precipitation, in Fifth International Iron and Steel Congress, Process Technology Proceedings, pp. 767–775 (1986)
4. M. Filipovic, C. Eriksson, H. Overstam, Behaviour of surface defects in wire rod rolling. Steel Res. Int. 77(6), 439–444 (2006)
5. J.Y. Kim, Y.G. Cho, Y.H. Kim, K.H. Lim, Y.S. Lee, The influence of roll caliber design on the wire rods wrinkle defect, in Proceedings of Exploitation of Future Rolling Technologies. Korea, pp. 180–187 (1999)