1. H. M. Nykyforchyn, O. Z. Student, and A. D. Markov, “Abnormal behavior of high-temperature degradation of the weld metal of low-alloy steel welded joints,” Fiz.-Khim. Mekh. Mater., 43, No. 1, 73–79 (2007); English translation: Mater. Sci., 43, No. 1, 77–84 (2007).
2. H. Nykyforchyn, E. Lunarska, O. Tsyrulnyk, et al., “Effect of the long-term service of the gas pipeline on the properties of the ferrite–pearlite steel,” Mat. Corr., 60, No. 9, 716–725 (2009).
3. H. Nykyforchyn, E. Lunarska, O. Tsyrulnyk, et al., “Environmentally assisted “in-bulk” steel degradation of long term service gas trunkline,” Eng. Failure Anal., 17, 624–632 (2010).
4. E. I. Kryzhanivs’kyi and H. M. Nykyforchyn, “Specific features of hydrogen-induced corrosion degradation of steels of gas and oil pipelines and oil storage reservoirs,” Fiz.-Khim. Mekh. Mater., 47, No. 2, 11–20 (2011); English translation: Mater. Sci., 47, No. 2, 127–136 (2011).
5. O. E. Andreikiv, O. V. Hembara, O. T. Tsyrul’nyk, and L. I. Nyrkova, “Evaluation of the residual lifetime of a section of a main gas pipeline after long-term operation,” Fiz.-Khim. Mekh. Mater., 48, No. 2, 103–110 (2012); English translation: Mater. Sci., 48, No. 2, 231–238 (2012).