1. P. O. Maruschak, A. P. Sorochak, and I. V. Konovalenko, “Stereoscopic analysis of the stretch zone of a steel specimen cut out of a railway axle and tested for static fracture toughness,” J. Fail. Anal. Prevent., 15, No. 3, 436–440 (2015).
2. E. V. Kharchenko, L. K. Polishchuk, and O. I. Zvirko "Estimation of the in-service degradation of steel shapes for the boom of a clamp-forming machine," Fiz.-Khim. Mekh. Mater., 49, No. 4, 77-82 (2013)
3. English translation: Mater. Sci., 49, No. 4, 501-507 (2014).
4. O. Zvirko, G. Gabetta, O. Tsyrulnyk, and N. Kret, “Assessment of in-service degradation of gas pipeline steel taking into account susceptibility to stress corrosion cracking,” Proc. Struct. Integrity, 16, 121–125 (2019).
5. H. Nykyforchyn, E. Lunarska, O. Tsyrulnyk, K. Nikiforov, and G. Gabetta, “Effect of the long-term service of the gas pipeline on the properties of the ferrite-pearlite steel,” Mat. Corr., 60, No. 9, 716–725 (2009).