1. M. Varga and M. Steltz, “Ten years of protective bricks ALUBAR — ten years of effective electrolyzer operation,” Alyuminii Sibiri, 106–107 (2005).
2. M. Sorley and H. Oiya, Cathodes in Aluminum Electrolyzer [Russian translation], Izd. Krasnoyarsk Univ., Krasnoyarsk (1997).
3. O.-J. Siljan, T. Grande, and C. Schoning, “Refractories for aluminum electrolysis cells. Part. I. Deterioration mechanisms based on phase equilibria,” ALUMINIUM, 77, No. 4, 294–300 (2001).
4. O.-J. Siljan, T. Grande, and C. Schoning, “Refractories for aluminum electrolysis cells. Part. II. Physical properties of penetrating melt, reduction by metals and volatile fluorides,” ALUMINIUM, 77, No. 5, 385–390 (2001).
5. O.-J. Siljan, T. Grande, and C. Schoning, “Refractories for aluminum electrolysis cells. Part. III. Laboratory tests cryolite resistance,” ALUMINIUM, 77, No. 7/8, 610–615 (2001).