1. V. V. Sharapova, I. I. Lishchuk, D. Yu. Boguslavskii, and V. V. Chesnyak, “Part 1. Mineral composition and phase transformations in the refractory lining of the bottom of aluminum electrolysis cells,” Novye Ogneupory, No. 3, 13–17 (2005).
2. D. V. Pruttskov, I. M. Bastryga, T. F. Raichenko, et al., “Phase transformations in the chamotte brick of the base plate of an aluminum electrolysis cell,” Tsvetn. Met., No. 11, 41–43 (1986).
3. D. V. Pruttskov, A. B. Bukher, V. P. Pirozhkova, Yu. I. Rys'eva, V. E. Pruttskov, A. P. Khvalin, and S. N. Dotsenko, “A mechanism of failure of the lining of an aluminum electrolysis cell,” Zh. Prikl. Khim., No. 1, 61–66 (1986).
4. D. V. Pruttskov, P. I. Titaev, A. A. Andriiko, and V. P. Pirozhkova, “The cryolite-nepheline state diagram and thermodynamic activity of its components,” Ukr. Khim. Zh., 56(5), 470–475 (1990).
5. G. N. Kozhevnikov and A. G. Vodop'yanov, The Lower Oxides of Silicon and Aluminum for Electrometallurgy [in Russian], Nauka, Moscow (1977).