1. AASHTO (1986) Standard method of test. mineral filler for bituminous paving mixtures. AASHT00O Designation: M17-83, Part I Specifications, 14th Edition.
2. ACI Committee 229 (1999) Controlled low-strength materials. American Concrete Institute. Farmington Hills, USA, p. 15
3. Al-Harthy AS, Taha R, Al-Maamary F (2003) Effect of cement kiln dust (CKD) on mortar and concrete mixtures. Construction and Building Materials 17 (5): 353–360.
4. Amin AM, Ebied E, El-Didamony H (1995) Activation of granulated slag with calcined cement kiln dust. Silicates Industrial 60 (3–4): 109–115.
5. Anil M, Upadhyaya S, Gustin F, Roohanirad A, Stokes J (2005) Full-depth cold in-place recycling of asphalt pavements with self-cementing fly ash: Field and laboratory studies. World of Coal Ash 2005; Lexington, Kentucky, USA.