1. Schubert, F., Bruch, U., Cook, R., Diehl, H., Ennis, P., Jakobeit, W., Penkalla, H., Heesen, E., Ullrich, G.: Creep rupture behavior of candidate materials for nuclear process heat applications. Nucl. Technol. 66(2), 227–240 (1984). https://doi.org/10.13182/NT84-A33426
2. Shariat, M., Faraji, A., AshrafRiahy, A., Alipour, M.: In advanced creep failure of H.P. modified reformer tubes in an ammonia plant. J. Corros. Sci. Eng. 6, 20 (2003)
3. Stevens, K., Trompetter, W.: Calibration eddy current carburization measurements in ethylene production tubes using ion beam analysis. J. Phys. D Appl. Phys. 37(3), 501–509 (2004). https://doi.org/10.1088/0022-3727/37/3/031
4. Jasiński, W., Zawada, P.: The precipitation processes in the Manaurite XM superalloy during 1000 hours of ageing. Int. J. Microstruct. Mater. Prop. 3(4–5), 607–615 (2008). https://doi.org/10.1504/IJMMP.2008.022039
5. Mathieu, S., Aranda, L., Portebois, L., Mathieu, S., Vilasi, M.: On the pre-oxidation treatments of four commercial Ni-based superalloys in air and in Ar–H2O at 950 °C. Oxid. Met. 90(1–2), 43–63 (2018). https://doi.org/10.1007/s11085-017-9822-5