Author:
Emmanuel Max,Gavalda-Diaz Oriol,Sernicola Giorgio,M’saoubi Rachid,Persson Tomas,Norgren Susanne,Marquardt Katharina,Britton T. Ben,Giuliani Finn
Abstract
AbstractThe grain boundary network of WC in WC-Co is important, as cracks often travel intergranularly. This motivates the present work, where we experimentally measure the fracture energy of Σ2 twist grain boundaries between WC crystals using a double cantilever beam opened with a wedge under displacement control in a WC-10wt%Co sample. The fracture energy of this boundary type was compared with cleaving {$$10\overline{1}0$$
10
1
¯
0
} prismatic planes in a WC single crystal. Fracture energies of 7.04 ± 0.36 Jm−2 and 3.57 ± 0.28 Jm−2 were measured for {$$10\overline{1}0$$
10
1
¯
0
} plane and Σ2 twist boundaries, respectively.
Publisher
Springer Science and Business Media LLC
Subject
General Engineering,General Materials Science
Reference39 articles.
1. R.E. Krebs, The History and use of our Earth’s Chemical Elements: A Reference Guide, 2nd edn. (Greenwood, Westport, 2006), p 154.
2. M. Srinivasan, and W. Rafaniello, Carbide, Nitride and Boride Materials Synthesis and Processing, 1st edn. (Chapman & Hall, London, 1997), pp 10–12.
3. K. Ravichandran, Acta Metall. Mater. 42, 143. (1994).
4. L.S. Sigl, and H.F. Fischmeister, Acta Metall. 36, 887. (1988).
5. L. Llanes, Y. Torres, and M. Anglada, Acta Mater. 50, 2381. (2002).
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献