1. Chen ST, Jiang ZH, Wu YY, Yang HY (2011) Development of a grinding–drilling technique for holing optical grade glass. Int J Mach Tools Manuf 51:95–103
2. Denisenko ET, Voinitskii AG, Polushko AP, Kostenko AD, Filatova NA (1970) Some deformation characteristics of copper containing oxide inclusions. Probl Prochn 11:54–57
3. Denisenko ET, Polushko AP, Filatova NA, Kostenko AD (1971) Effect of various factors on the properties of copper hardened with dispersed oxides. Poroshk Metall 10:49–54
4. Fedorchenko IM, Denisenko ET, Sakhnenko AV, Polushko AP, Perepelkin AV (1974) Bulk forging technology and properties of dispersion-strengthened copper electrode materials. Transactions of the fourth international conference on powder metallurgy in Czechoslovakia, pp 171–187
5. Kobayashi KF, Tachibana N, Shingu PH (1990) Formation of amorphous Al–Cr alloys by mechanical alloying of elemental aluminium and chromium powders. J Mater Sci 25:3149–3154