Abstract

The use of non-destructive examination (NDE) for assessing the quality of butt fusion joints in polyethylene (PE) pipes has been included in the draft Mandatory Appendix XXVI to Section III of the ASME Boiler and Pressure Vessel Code (Rules for construction of Class 3 buried polyethylene pressure piping). However, currently, there are no acceptance criteria for flaws in butt fusion joints in PE pipes. There is an ASME Task Group on flaw evaluation for PE pipe, which is developing a code case using linear elastic fracture mechanics (LEFM) to determine critical flaw sizes. However, the initial experimental crack growth data generated suggests that linear elastic fracture mechanics is not able to adequately describe slow crack growth in PE materials. In addition, this work is only considering planar lack of fusion flaws in the joint; it is not considering other critical flaw types that can occur in butt fusion joints, such as particulate contamination and cold fusion. TWI has developed procedures using mechanical testing to develop flaw acceptance criteria for butt fusion joints in PE pipes. This is based on inserting lack of fusion flaws of known size and particulate contamination flaws of known concentrations into butt fusion joints and determining the effect of these flaws on both the short-term and long-term integrity of the joints. An important aspect of this work is to determine which of the wide array of mechanical tests available for assessing the integrity of butt fusion joints in PE pipes are the most discriminating. This paper describes the procedures developed for inserting simulated flaws into butt fusion joints in PE pipes, the experimental work to compare the results from different standard short-term and long-term tests on flawed and unflawed joints and the procedures developed to determine flaw acceptance criteria. Results have shown that the most discriminating short-term test for butt fusion joints in PE pipes is a tensile test using a waisted specimen, such as those defined in EN 12814-2, EN 12814-7 and ISO 13953, and the most discriminating property is the energy to break the specimen. The most appropriate long-term test for butt fusion joints in PE pipes is the whole pipe tensile creep rupture test, as defined in EN 12814-3; this is the only long-term whole pipe test that consistently generates slow crack growth in the fused joint, even if it contains no flaws.

Publisher

American Society of Mechanical Engineers

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3