Abstract

The American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (Code) provides rules for the design of Class 1 components of nuclear power plants. However, the Code design curves do not address the effects of light water reactor (LWR) water environments. Existing fatigue strain-versus-life (ε–N) data illustrate significant effects of LWR water environments on the fatigue resistance of pressure vessel and piping steels. Extensive studies have been conducted at Argonne National Laboratory (Argonne) and elsewhere to investigate the effects of LWR environments on the fatigue life. This article summarizes the results of these studies. The existing fatigue ε–N data were evaluated to identify the various material, environmental, and loading conditions that influence the fatigue crack initiation; a methodology for estimating fatigue lives as a function of these parameters was developed. The effects were incorporated into the ASME Code Section III fatigue evaluations in terms of an environmental correction factor, Fen, which is the ratio of fatigue life in air at room temperature to the life in the LWR water environment at reactor operating temperatures. Available fatigue data were used to develop fatigue design curves for carbon and low-alloy steels, austenitic stainless steels (SSs), and nickel–chromium–iron (Ni–Cr–Fe) alloys and their weld metals. A review of the Code Section III fatigue adjustment factors of 2 and 20 is also presented, and the possible conservatism inherent in the choice is evaluated. A brief description of potential effects of neutron irradiation on fatigue crack initiation is presented.

Funder

U.S. Nuclear Regulatory Commission

Publisher

ASME International

Subject

Mechanical Engineering,Mechanics of Materials,Safety, Risk, Reliability and Quality

Reference149 articles.

1. Hale, D. A., Wilson, S. A., Kiss, E., and Giannuzzi, A. J., 1977, “Low-Cycle Fatigue Evaluation of Primary Piping Materials in a BWR Environment,” U.S. Nuclear Regulatory Commission, Washington, DC, Report No. GEAP-20244.

2. Low Cycle Fatigue Behavior of Commercial Piping Materials in a BWR Environment;J. Eng. Mater. Technol.,1981

3. Ranganath, S., Kass, J. N., and Heald, J. D., 1982, “Fatigue Behavior of Carbon Steel Components in High-Temperature Water Environments,” BWR Environmental Cracking Margins for Carbon Steel Piping, Electric Power Research Institute, Palo Alto, CA, Report No. EPRI NP-2406, Appendix 3.

4. Fatigue Behavior of Carbon Steel Components in High-Temperature Water Environments,1982

5. JNES-SS Report, 2011, “Environmental Fatigue Evaluation Method for Nuclear Power Plants,” Nuclear Energy System Safety Division, Japan Nuclear Energy Safety Organization, Tokyo, Japan, Report No. JNES-SS-1005.https://www.nrc.gov/docs/ML1130/ML113010189.pdf

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3