Stress Distribution in Metal-Ceramic Crowns with a Facial Porcelain Margin

Author:

Anusavice K.J.1,Hojjatie B.1

Affiliation:

1. Department of Dental Biomaterials, College of Dentistry, University of Florida, Gainesville, Florida 32610

Abstract

The use of metal-ceramic restorations with porcelain butt-joint facial margins has increased in the past several years. Although these crowns exhibit improved esthetics compared with metal-ceramic crowns which display a metal gingival collar or metal knife-edge margin, the effectiveness of this design in resisting intra-oral forces is not known. The objective of this study was to analyze the stress distribution induced by simulated intra-oral loads on crowns with variable coping configurations. The copings, with a thickness of either 0. 1 or 0.3 mm, were modeled with a facial termination of metal at three locations: at the gingival floor, 0.9 mm above the gingival floor, and 4.2 mm above the gingival floor. The coping and crown dimensions were based on a prepared maxillary central incisor with a facial shoulder and a lingual chamfer. Both Ni-Cr and Au-Pd alloy copings were employed in the crown models. Finite element stress analyses were performed on crowns which were subjected to several loading conditions. A cement film thickness of 0.030 mm was assumed. For all cases, the stresses which developed in porcelain and cement near the facial and lingual margins due to a vertical load of 200 N were predominately compressive in nature. For the crowns with Ni-Cr copings, the tensile stress in porcelain ranged from 11.0 MPa (for crowns with a facial metal thickness of 0.3 mm) to 12.5 MPa (for a metal thickness of 0.1 mm). The corresponding stresses for crowns with Au-Pd alloy copings were 8.3 MPa and 8.6 MPa, respectively. Maximum compressive stresses in cement near the lingual margin were 22.3 MPa for the Ni-Cr crowns and 30.0 MPa for the Au-Pd crowns. The maximum tensile stress in porcelain was 29.0 MPa and occurred near the area of loading for the Au-Pd case. The maximum tensile stress in the facial porcelain region (8.3 MPa) developed within the incisal third of the facial surface. Under the conditions assumed in this study, the alloy type, coping thickness, and coping termination point have a negligibly small effect on the stresses induced in porcelain or cement near the facial margin.

Publisher

SAGE Publications

Subject

General Dentistry

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3