Abstract
The cracking thresholds were evaluated for tungsten samples with different microstructure in the course of QSPA Kh-50 repetitive plasma loads. No damage has been observed on the exposed surfaces under 0.1 MJ/m2. Nevertheless, cracks were detected in the bulk of irradiated tungsten (with longitudinal grain orientation). Increasing heat load up to 0.2 MJ/m2 caused the damaging of all types of tungsten targets. The observed cracks propagate to the bulk mainly transversely and parallel to the irradiated surface. The effect of the subsequent exposure with LHD divertor plasma on the tungsten samples was analyzed. The obtained results are discussed.
Publisher
Problems of Atomic Science and Technology
Reference16 articles.
1. S. Brezinsek et al. // Nuclear Fusion. 2017, v. 57, p. 116041.
2. T. Hirai et al. // Nuclear Materials and Energy. 2016, v. 9, p. 616-622.
3. Q. Zhou et al. // Fusion Engineering and Design. 2020, v. 159, p. 111879.
4. S. Pestchanyi et al. // Fusion Eng. Design 2011, v. 86, 9-11, p. 1681-1684.
5. I.E. Garkusha et al. // Fusion Science and Technology. 2014, v. 65(2), p. 186-193.
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献