Objective: To study the fracture resistance and failure modes of different type of ceramic crowns. Methods: Four groups of crown including zirconia-veneering porcelain crown (Group 1), whole zirconia crown (CAD/CAM, Group 2), cast ceramic crown (Group 3) and glass ceramic crown (CAD/CAM, chairside, Group 4) with the same thickness were manufactured, each group own 12 crowns. The fracture resistance test and failure modes analysis of the specimens were conducted, SPSS22.0 was used to analyze the difference among the groups. Results: The fracture strength of Group 2 is significantly higher than other three group (P<0.05), Statistical significance was found between group 3 and group 1, group 4. No Statistical significance was found between group 1 and group 4. The failure modes of the whole zirconia crown, the cast ceramic crown and the glass ceramic crown are complete crown fracture; 33% of the zirconia-veneering porcelain crown showed veneering layer fracture, the other 67% showed complete crown fracture. Conclusion: The fracture resistance of the whole zirconia crown are higher than the cast ceramic crown, the zirconia-veneering crown and the glass ceramic crown and the glass ceramic crown (CAD/CAM) is a very convenient prostheses. The failure modes are significantly influenced by the type of the crown.
Publisher
Trans Tech Publications, Ltd.
Subject
Condensed Matter Physics,General Materials Science,Atomic and Molecular Physics, and Optics
Reference11 articles.
1. Alaa M. Attaallah, Eman M Zayed, Salma M Dabees, et al. Comparison between Biaxial Flexural Strength and Microstructure of Polished and Glaze-Fired Specimens of Zirconia Lithium Silicate Glass Ceramic. Journal of Dental Materials and Techniques, 2019, 8(3): 114-120.
2. Jasim HH, Findakly MB, Mahdi NA, et al. Effect of Reduced Occlusal Thickness with Two Margin Designs on Fracture Resistance of Monolithic Zirconia Crowns. Eur J Dent. 2020, 14(2): 245-249.
3. Yousif Ezzat, Mohammed Al-Rafee. Effect of veneering material and technique on the fracture resistance of porcelain-veneered zirconia crowns. Saudi Journal of Oral Sciences, 2020, 7(1): 11-17.
4. Mores RT, Borba M, Corazza PH, et al. Influence of surface finishing on fracture load and failure mode of glass ceramic crowns. J Prosthet Dent. 2017, 118(4): 511-516.
5. Bergamo ETP, Bordin D, Ramalho IS, et al. Zirconia-reinforced lithium silicate crowns: Effect of thickness on survival and failure mode. Dent Mater. 2019, 35(7): 1007-1016.