The investigations of (Ti + Al)-SiO2 surfacing by magnetron deposition are presented in this article. The correlation between film`s thickness deposited on the particles by mechanocomposites and magnetron sputtering time was established. It was determined that the rational time for surfacing by Ti-Al mechanocomposites system is about 40 minutes. According that deposition time the thickness of deposited SiO2 films were obtained as 5.2 microns.
Publisher
Trans Tech Publications, Ltd.
Subject
Condensed Matter Physics,General Materials Science,Radiation
Reference24 articles.
1. K.S. Vecchio, Synthetic multifunctional metallic-intermetallic laminate composites, The Journal of The Minerals. 57 (2005) 25-31.
2. M. Palm, L.C. Zhang, F. Stein, G. Sauthoff, Phases and phase equilibria in the Al rich part of the Al-Ti system above 900C, Intermetallics. 10 (2002) 523-540.
3. R. Przeliorz, M. Goral, G. Moskal, L. Swadzba, The relationship between specific heat capacity and oxidation resistance of TiAl alloys, Journal of Achievements of Materials and Manufacturing Engineering. 21 (2007) 48-50.
4. A. Rohatgi, D.J. Harach, K.S. Vecchio, K.P. Harvey, Resistance-curve and fracture behavior of Ti-Al3-Ti metallic intermetallic laminate (MIL) composites, Acta Materialia. 51 (2003) 2933-2957.
5. F.J.J. van Loo, G.D. Rieck, Diffusion in the titanium-aluminium system - II. Interdiffusion in the composition range between 25 and 100 at.% Ti, Acta Metallurgica. 21(1) (1973) 73-84.