Affiliation:
1. Rajapark Institute
2. King Mongkut’s University of Technology
Abstract
This study investigated characteristics of moisture desorption for polylactic acid (PLA) filaments. The filaments tend to absorb moisture from humid air, led to moisten filaments. The absorption of even small amounts of moisture by filaments during storage and/or 3D printing, degraded the quality of final parts, and therefore, caused manufacturing problems. In this work, the filaments were subjected to humid conditions to achieve various moisture concentrations (0.75, 1.3 and 1.87 wt.%). Warm air-drying processes are used to reduce the moisture for different times (1, 2, 3, 4, 5 and 6 hours) and temperature (40, 50 and 60 °C). It was founded that the moisture from the polylactic acid (PLA) filaments can be discovered the moisture by use 60 degree of temperature in 5 hours warm air-drying process.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献