Affiliation:
1. Hebei United University
2. Beijing General Research Institute for Nonferrous Metals
Abstract
Heat-resistant Al-8.5Fe-1.3V-1.7Si aluminum alloys were prepared by spray forming technique. The phase transition of deposited alloys from room temperature to 500°C was measured by Differential Scanning Calorimeter. The organization and the second phases of the alloys were observed and studied by transmission electron microscopy. The research results show that No endothermic peak appears in the deposited alloys during heating process, there is no phase transition occur in the alloy during the heating process from room temperature to 500°C. The deposited alloys mainly include α-Al and α-Al12(Fe,V)3Si phase. Under the transmission electron microscopy, there are also a small amount of slug, fan-shaped, needle-like, block, strip second phases, these phases are Al12Fe3Si, Al8Fe2Si, θ-Al13Fe4, Al9FeSi3, Al6Fe.
Publisher
Trans Tech Publications, Ltd.
Reference7 articles.
1. ZHAN Mei-yan, XIA Wei-jun, ZHANG Hui, et al. Flow Stress Behavior of FVS0812 Heat-resistant Aluminum alloy Prepared by a Spray Dep0siti0n-extrusi0n Route Under Hot-compression Deformation[J]. Journal of Hunan University of Science & Technology, 2004, 19(2): 37-41.
2. Subhash C K, Alan L Y, Michael J K. Creep and microstructure stability of dispersion strengthened Al-Fe-V-Si-Er alloy[J]. Materials Science and Engineering A, 1993, 167(1-2): 11~21.
3. Lee J C, Lee S, Lee P Y, et al. The brittleness of a rapidly solidified Al-Fe-V-Si alloy after high-temperature exposure[J]. Metallurgical Transactions A, 1991, 22: 853~858.
4. Park W J, Ahn S, Nack J. Evolution of microstructure in a rapidly solidified Al-Fe-V-Si alloys[J]. Materials Science and Engineering A, 1994, 189: 291~299.
5. SUN Yu-feng, REN Chen-xing, SHEN Ning-fu, et al. Study on the microstructure Evolution of Spray Deposited Al-Fe-V-Si Alloy. Journal of Zhengzhou University of Technology[J], 2001, 22(4): 17-21.