Abstract
Four different heat treatment routes which were called step quenching were taken and accordingly different morphology dual-phase samples have been obtained. It is found that Maximum shear stress increases with martensite volume increases. They have the following relationship: Maximum shear stress = 1.14(MVF)2 – 90.7(MVF) + 24266 MPa. Adiabatic shear bands and cracks led by them are important signs during the dynamic torsional tests
Publisher
Trans Tech Publications, Ltd.
Reference13 articles.
1. W. C. Leslie, The Physical Metallurgy of Steels, 1981, 162.
2. D.J. Bailey and R. Stevenson, Met. Trans. A, 10A: 47(1979).
3. R. Stevenson, D.J. Bailey, and G. Thomas, Met. Trans. A, 10A: 57(1979).
4. H.J. Klaar, I.A. El-Sesy, A.A. Hussein, Steel Res. 61 (2) (1990).
5. A. Bag, K.K. Ray, E.S. Dwarakadasa, Metall. Trans., A 30(1999) 1193– 1202.