Carbon steel and stainless steel equipment exposed to gas mixtures rich in hydrogen and carbon-monoxide at temperatures from 800 to 1200 F have been attacked with resulting loss of metal. Conditions under which this attack has been observed in a coal-to-oil synthesis plant and the nature of metal deterioration are described, Mechanism of this type attack is not fully understood although a possible gas-metal reaction is postulated. 3.2.2