Abstract
Oxidation of silicon carbide (SiC) is known to induce defects at the interface of the SiO2/SiC system. NO-annealing is a standard industrial method of nitridation, but oxidation may progress during NO-nitridation, which may generate interface defects. Here, we propose a new method of fabricating SiO2/SiC metal-oxide-semiconductor (MOS) devices: sputter deposition of SiO2 in an Ar/N2 gas mixture followed by high-temperature CO2-post deposition annealing to form SiO2 and incorporate nitrogen at the interface while suppressing oxidation of the SiC. We obtained the nitrogen depth profile by performing x-ray photoelectron spectroscopy and confirmed that most of the nitrogen atoms exist at the abrupt interface. While maintaining a low interface state density and good insulating property, we demonstrated much improved reliability of MOS devices compared to conventional NO-annealed samples, thanks to the well-designed SiO2/SiC interface by the proposed method.
Funder
Ministry of Education, Culture, Sports, Science and Technology
Japan Society for the Promotion of Science
Subject
General Physics and Astronomy
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献