Abstract
Abstract
Background
The purpose of the study is to analyse the effects of different inhaled asthma medications (IAMs) on the color change of dental restorative materials (DRMs).
Methods
In total, 192 samples were taken from six different DRMs: [Filtek Z550 (nanohybrid composite), Fusio Liquid Dentin (Self-adhering flowable composite), Filtek Ultimate (nanofilled flowable composite), Dyract XP (compomer), Fuji II LC (resin-modified glass ionomer), Fuji IX Fast (self-cured-packable glass ionomer), (n = 32)]. After the initial color values (CIELab) of DRMs were measured by using a spectrophotometer, each sample was exposed to the same IAMs via nebulizer according to the four different inhaled therapies and measurements were repeated on the 7th & 21st days.
Results
In all IAM groups, DRM with the least amount of ΔE was nanohybrid composite, while the highest ΔE was found in Fuji II LC. Among all experimental groups, only Fuji II LC which was administered the combined medication, exceeded the clinically unacceptable threshold (ΔE = 3.3) on 7th & 21st days.
Conclusions
Consequently, important factors affecting the susceptibility to color stability are the type of IAMs, the administration time-dosage, and the type of DRMs.
Funder
Sivas Cumhuriyet University Scientific Research Projects
Publisher
Springer Science and Business Media LLC
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献