Author:
Gurtovoi V. G.,Sheleg A. U.,Guretskii S. A.
Subject
Materials Chemistry,Metals and Alloys,Inorganic Chemistry,General Chemical Engineering
Reference7 articles.
1. Abrahams, S.C., Jamieson, P.B., and Bernstein, J.L., Ferroelectric Tungsten Bronze-Type Crystal Structures: III. Potassium Lithium Niobate K6−x−y Li4+x Nb10+y O30, J. Chem. Phys., 1971, vol. 54, no. 6, pp. 2355–2364.
2. Li, L., Chong, T.C., Xu, X.W., et al., Growth of Potassium Lithium Niobate (KLN) Single Crystals for Second Harmonic Generation (SHG) Application, J. Cryst. Growth, 2000, vol. 211, p. 281.
3. Kim, J.S. and Lee, H.J., Growth and Properties of Ferroelectric Potassium Lithium Niobate (KLN) Crystal Grown by the Czochralski Method, J. Cryst. Growth, 2001, vol. 223, pp. 376–382.
4. Kang, G.Y. and Yoon, J.K., The Growth of Potassium Lithium Niobate (KLN) with Low Nb2O5 Content, J. Cryst. Growth, 1998, vol. 193, pp. 615–622.
5. Ramirez, A.P., Lawes, G., Butko, V., et al., Colossal Dielectric Constants in Braced Lattices with Defects, Eprint, cond-mat/0 209 498, 2002 ( http://arxiv.org/pdf/cond-mat/0209498 ).