Abstract
AbstractWhile glass alteration in liquid water has been widely studied for decades, glass alteration in unsaturated atmosphere (relative humidity, RH < 100%) has been far less examined. However, the understanding of the mechanisms involved in the reactions between glass and water in vapor state is fundamental to several fields such as glass industry, conservation of glasses of the cultural heritage and long-term assessment of nuclear waste glasses. This paper outlines the issues raised by the atmospheric alteration of glass in these fields and attempts to summarize the scientific approaches and findings of the three communities. This short review reveals that atmospheric alteration should not be confused with liquid alteration at high S/V (S = exposed surface of glass and V = volume of solution), because the kinetics and the nature of the alteration products are distinct. Notably, alkalies and non-bridging oxygens may be significantly retained in glass hydrated in unsaturated atmosphere, depending on the glass composition. Future lines of research are drawn to progress in the understanding of the specificities of atmospheric glass alteration.
Publisher
Springer Science and Business Media LLC
Subject
Materials Chemistry,Materials Science (miscellaneous),Chemistry (miscellaneous),Ceramics and Composites
Reference116 articles.
1. Kunicki-Goldfinger, J. J. Unstable historic glass: symptoms, causes, mechanisms and conservation. Rev. Conserv. 9, 47–60 (2008).
2. Werme, L. et al. Chemical corrosion of highly radioactive borosilicate nuclear waste glass under simulated repository conditionso Title. J. Mater. Res. 5, 1130–1146 (1990).
3. Bates, J. K. et al. High-Level Waste Borosilicate Glass: A Compendium of Corrosion Characteristics. Vol. 1. DOE-EM-0177 (1994).
4. Organ, R. M. The safe storage of unstable glass. Mus. J. 56, 255–272 (1957).
5. Brill, R. H. Crizzling—a problem in glass conservation. Stud. Conserv. 20, 121–134 (1975).
Cited by
51 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献