Abstract
ABSTRACTThe liquidus temperature (TL) often limits the loading of
high-level waste in glass through the constraint that TL must be
at least 100°C below the temperature at which the glass viscosity is 5 Pa-s.
In this study, values of TL for spinel primary crystalline phase
were measured as a function of glass composition. The test glasses were
based on high-iron Hanford Site tank wastes. All studied glasses
precipitated spinel (Ni,Fe,Mn)(Cr,Fe)2O4 as the
primary crystalline phase. TL was increased by additions of
Cr2O3, NiO, Al2O3,
Fe2O3, MgO, and MnO; while Li2O,
Na2O, B2O3, and SiO2 had a
negative effect. Empirical mixture models were fitted to data.