Abstract
The wear of enamel and crown restorative materials often occur by occlusion. The purpose of this study was to evaluate the wear volume between glass-ceramics used for CAD/CAM blocks (lithium disilicate: Initial LiSi block (LIS), IPS e.max CAD (IPS), zirconia-reinforced lithium silicate glass-ceramics: Celtra DUO (DUO), VITA Suprinity (VITS) and feldspar-based glass-ceramics: Vitablocs Mark II (MAK)) and bovine tooth enamel using a two-body wear test, the hardness, three-point bending strength, micro-structure and the element components of glass-ceramics. The data were analyzed using a one-way analysis of variance and Tukey’s multiple comparison test (α = 0.05). IPS and DUO with relatively large size crystal gain had significantly larger abrader wear volumes. Zirconia-reinforced lithium silicate glass-ceramics (DUO, VITS) caused significantly greater wear volume in antagonist enamel. MAK with scale-shape crystals grains produced distinct scratches after wear tests, both in the material itself and in the enamel. A strong correlation between the mechanical properties (hardness, three-point bending strength) and wear volume could not be confirmed. The type of glass-ceramic, size, and shape of the crystal grains affected the wear behavior of the glass-ceramics for CAD/CAM blocks. Therefore, dentists should consider that wear behavior varies with crystal structure, size, and shape in glass-ceramics for CAD/CAM blocks.
Subject
General Materials Science
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献