Abstract
Understanding and characterizing crack growth is central to meeting the damage tolerance and durability requirements delineated in USAF Structures Bulletin EZ-SB-19-01 for the utilization of additive manufacturing (AM) in the sustainment of aging aircraft. In this context, the present paper discusses the effect of different AM processes, different build directions, and the variability in the crack growth rates related to AM Ti-6Al-4V, AM Inconel 625, and AM 17-4 PH stainless steel. This study reveals that crack growth in these three AM materials can be captured using the Hartman–Schijve crack growth equation and that the variability in the various da/dN versus ΔK curves can be modeled by allowing the terms ΔKthr and A to vary. It is also shown that for the AM Ti-6AL-4V processes considered, the variability in the cyclic fracture toughness appears to be greatest for specimens manufactured using selective layer melting (SLM).
Subject
General Materials Science
Reference43 articles.
1. Directive-type Memorandum (DTM)-19-006—Interim Policy and Guidance for the Use of Additive Manufacturing (AM) in Support of Materiel Sustainment,2019
2. Additively manufactured Ti-6Al-4V replacement parts for military aircraft
3. Structures Bulletin EZ-SB-19-01, Durability and Damage Tolerance Certification for Additive Manufacturing of Aircraft Structural Metallic Parts,2019
Cited by
30 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献