Abstract
Waterlogged archaeological wood samples may degrade during long-term immersion in microbial-activity environments, which causes its biodegradation. Simultaneous dynamic vapor sorption (SDVS) and two-dimensional correlation infrared (2D COS-IR) spectroscopy reveal the degradation inhomogeneity of waterlogged fir wood from the Shengbeiyu shipwreck. The waterlogged and reference wood exhibit type II sorption isotherms. The equilibrium moisture contents of waterlogged archaeological fir wood from a decay region (WFD) were 22.5% higher than those of waterlogged archaeological fir wood from a sound region (WFS). WFD exhibits a higher measurable sorption hysteresis than WFS, implying greater variation in the surface moisture content in the WFD region compared to the WFS region, which may compromise the dimensional stability of the shipwreck. 2D COS-IR spectra confirmed the inhomogeneous degradation of the waterlogged wood via numerous mechanisms. The efficacy of SDVS and 2D COS-IR spectroscopy in the evaluation of the degradation state of waterlogged wood was demonstrated. This study verifies the existence of hygroscopic and chemical differences between visually similar samples from the same shipwreck.
Funder
National Key Research and Development Program of China
China Postdoctoral Science Foundation
fundamental research funds for the central universities
Reference69 articles.
1. Broda, M., and Hill, C.A.S. (2021). Conservation of Waterlogged Wood—Past, Present and Future Perspectives. Forests, 12.
2. Håfors, B. (2010). Conservation of the Wood of the Swedish Warship Vasa of AD 1628. Evaluation of Polyethylene Glycol Conservation Programmes, Department of Conservation, Gothenburg University.
3. Han, L.Y., Guo, J., Wang, K., Gronquist, P., Li, R., Tian, X.L., and Yin, Y.F. (2020). Hygroscopicity of Waterlogged Archaeological Wood from Xiaobaijiao No.1 Shipwreck Related to Its Deterioration State. Polymers, 12.
4. The characterization of waterlogged archaeological wood: The three Roman ships found in Naples (Italy);Capretti;Archaeometry,2008
5. Conservation and in situ preservation of wooden shipwrecks from marine environments;Gregory;J. Cult. Herit.,2012
Cited by
9 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献