Abstract
This paper describes the use of Supersonic Laser Deposition (SLD) to manufacture nickel/graphite composite coatings on titanium and aluminium substrates. Laser heating is critical for depositing coatings containing up to 13.3 vol% graphite. For a given feedstock composition, the resulting graphite content and average size of the graphite particles retained in the coating increases with laser power, until substrate melting occurs. The effect of the powder type, feedstock composition, and process conditions on coating structure is characterized. The friction and wear behaviour of selected coating compositions is examined. Nickel coatings containing 13.3 vol% graphite demonstrated self-lubricating behaviour with a stable coefficient of friction below 0.14 in pin-on-disc testing.
Subject
Materials Chemistry,Surfaces, Coatings and Films,Surfaces and Interfaces
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献