Influence of Five Additives on No Loading Swelling Potential of Red Clay

Author:

Yue Bing,Zhao Ziye,Qian Zengzhen

Abstract

In this study, cement, zeolite powder and three industrial by-products (blast furnace slag, steel slag, and fly ash) were selected as additives to study their effects on the swelling potential of red clay with different curing ages and dosages. At the same time, the mechanism of additives reducing the swelling potential of red clay was analyzed by scanning electron microscope (SEM) and X-ray fluorescence (XRF) tests. The X-ray diffraction (XRD) test was used to detect the clay mineral content of the red clay specimens before and after the modification to determine the change in the clay mineral content of the specimens. The direct shear test was used to explore the influence of additives on the strength of red clay. The results show that with 9% cement content, the no loading swelling potential of specimens can be reduced by 82.5% under 28 days of curing, and the cohesion of the specimens can be greatly increased by 82%. However, the specimens with cement have an increase in no loading swelling potential under the condition of no curing. In contrast, when steel slag is used as an additive to modify the swelling properties of red clay, the swelling potential can be reduced without curing, but the addition of steel slag will reduce the cohesive strength of specimens. XRD testing shows that the clay mineral composition in cement-modified specimens and steel slag-modified specimens experienced a relative change, the relative content of montmorillonite and illite decreased, and the relative content of kaolinite increased. Combined with SEM and XRF test results, it is concluded that cement’s reduction in the swelling potential of red clay depends on pozzolanic reaction products filling the pores in specimens and bonding clay particles, so as to reduce the permeability of red clay and increase the resistance during swelling. The addition of cement can also convert hydrophilic clay minerals into nonhydrophilic clay minerals. Compared with cement, the reduction in swelling potential caused by steel slag mainly depends on the adsorption of ions to reduce the adsorption of water molecules on the surface of clay slices.

Publisher

MDPI AG

Subject

Fluid Flow and Transfer Processes,Computer Science Applications,Process Chemistry and Technology,General Engineering,Instrumentation,General Materials Science

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3