The aim of this work was synthesizing ester elastomers, using sorbitol as a monomer obtainable from renewable sources. Three polymers were synthesized, utilizing three different polycondensation times. Their mechanical and thermal properties were examined and compared. Poly(sorbitol sebacate-co-butylene sebacate) elastomers were synthesized as a result of polycondensation reaction, using sebacic acid, butylene glycol and sorbitol as monomers. Resulting materials had good mechanical properties and a cross-linked structure. Such elastomers are susceptible to hydrolytic degradation which has been confirmed in earlier studies. This paper shows that the material synthesized utilizing a 3.5 h polycondensation time has the most desirable mechanical and thermal properties, and the reaction is characterized by the highest degree of conversion of substrates.
Subject
Fluid Flow and Transfer Processes,Computer Science Applications,Process Chemistry and Technology,General Engineering,Instrumentation,General Materials Science
Cited by
12 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献